| (a) | low alloy steel | yield 1.2 GPa | toughness 70 MPa√m, |
| (b) | maraging steel | yield 1.8 GPa | toughness 50 MPa√m |
| (a) | tough, weak | yield 700 MPa | plane strain toughness 100 MPa√m |
| (b) | brittle, strong | yield 1400 MPa | plane strain toughness 50 MPa√m |
Multiple service failures occur when the deposition properties are as (b) below. Would a change to (a) or to (c) alleviate the problem ?
| deposition | (a) | (b) | (c) |
| yield ( MPa ) | 600 | 800 | 1000 |
| toughness ( MPa√m ) | 120 | 90 | 60 |